Thermo-mechanical fatigue of single crystal nickel-based superalloy DD8

โœ Scribed by F. Liu; Z.G. Wang; S.H. Ai; Y.C. Wang; X.F. Sun; T. Jin; H.R. Guan


Book ID
114387360
Publisher
Elsevier Science
Year
2003
Tongue
English
Weight
331 KB
Volume
48
Category
Article
ISSN
1359-6462

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES


Thermo-mechanical fatigue failure of a s
โœ M. Okazaki; M. Sakaguchi ๐Ÿ“‚ Article ๐Ÿ“… 2008 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 480 KB

Behavior of thermo-mechanical fatigue (TMF) of a single crystal Ni-based superalloy, CMSX-4, was studied, compared with that of isothermal low cycle fatigue (LCF). Strain-controlled TMF and LCF tests of CMSX-4 were carried out under various test conditions, where the experimental variables were stra