Effect of biomineralized manganese on pi
✍ B. H. Olesen; N. Yurt; Z. Lewandowski πŸ“‚ Article πŸ“… 2001 πŸ› John Wiley and Sons 🌐 German βš– 161 KB

During the past few years, biomineralized manganese has been shown to cause ennoblement of various stainless steels to open circuit potentials of 300 Β± 400 mV/SCE. We have demonstrated that ennoblement, caused by biologically deposited manganese minerals, along with a relatively low stainless steel

Pitting corrosion transformation of SUS3
✍ H.-X. Chen; X.-H. Ma; J.-B. Chen; S.-S. Bo πŸ“‚ Article πŸ“… 2009 πŸ› John Wiley and Sons 🌐 German βš– 207 KB

## Abstract The foundational data and rules of SUS304 corrosion in aqueous lithium bromide solution at 150–200 °C have been investigated by means of weight loss in this paper. The Taguchi method was chosen to investigate the effects of variables on corrosion at higher temperature. Concentration of