In this paper, we report all of the electro-optic coe cients of the low symmetry crystal GdCa4O(BO 3 ) 3 measured by the interferometric method. The new sample orientations, which have not been reported so far, have been used for measuring the skew electro-optic coe cients 51, 53, 42 and 62 independently. The results obtained are 11 = 0:4, 21 = 0:5, 31 = 0:6, 13 = 0:1, 23 = 0:4, 33 = 2:0


๐Ÿ“œ SIMILAR VOLUMES


Temperature behavior of piezoelectric ga
โœ Markiewicz, E. ;Pawlaczyk, C. ;Kล‚os, A. ;Hofman, W. ;Pajaฬจczkowska, A. ๐Ÿ“‚ Article ๐Ÿ“… 2006 ๐Ÿ› John Wiley and Sons ๐ŸŒ English โš– 201 KB

## Abstract Temperature characteristics of the piezoelectric resonance frequencies of gadolinium calcium oxoborate (GdCOB) were studied for the following crystal cuts and vibration modes: (__XYt__)__ฯ•__ (__ฯ•__=ย 0__ยฐ__, 22.5__ยฐ__, 67.5__ยฐ__) bars vibrating in longitudinal mode, (__XYt__)45ยฐ bar vibr

Growth and properties of (Cr3+, Nd3+) do
โœ Shujun Zhang; Zhenxiang Cheng; Guangyong Zhou; Yuming Sung; Xueyuan Hou; Xuesong ๐Ÿ“‚ Article ๐Ÿ“… 2000 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 646 KB

Optical quality Nd:GdCa40(BO3)3 (Nd:GdCOB) crystal and chromium sensitized crystal of Cr:Nd:GdCa40(BO3)3 (Cr:Nd:GdCOB) were grown by the Czochralski (CZ) method. The transmittance spectra was measured at room temperature on 7at%Nd:GdCOB and lat%Cr:7at%Nd:GdCOB samples. The absorption in the blue-UV

Elastic and piezoelectric properties of
โœ Pawlaczyk, C. ;Markiewicz, E. ;Kล‚os, A. ;Hofman, W. ;Pajaฬจczkowska, A. ๐Ÿ“‚ Article ๐Ÿ“… 2006 ๐Ÿ› John Wiley and Sons ๐ŸŒ English โš– 666 KB

## Abstract Gadolinium calcium oxoborate, GdCa~4~O(BO~3~)~3~ (GdCOB), single crystals were grown by the Czochralski technique. The orientation of crystal was precisely determined. To estimate the complete matrices of the elastic (13) and piezoelectric (10) coefficients measurements of the complex e