The synthesis of alkali substituted lanthanum copper oxide La2\_xMxCuO4 (M=Na, K, Rb, Cs) by the low temperature hydroxide melt technique is described. The alkali stoichiometry x turned out to be dependent upon the reaction temperature. Superconducting phases appear in the Na and K substituted compo
Low-temperature ferroelectric phase and magnetoelectric coupling in underdoped La_{2}CuO_{4+x}
✍ Scribed by Viskadourakis, Z.; Radulov, I.; Petrović, A. P.; Mukherjee, S.; Andersen, B. M.; Jelbert, G.; Headings, N. S.; Hayden, S. M.; Kiefer, K.; Landsgesell, S.; Argyriou, D. N.; Panagopoulos, C.
- Book ID
- 111918299
- Publisher
- The American Physical Society
- Year
- 2012
- Tongue
- English
- Weight
- 997 KB
- Volume
- 85
- Category
- Article
- ISSN
- 1098-0121
No coin nor oath required. For personal study only.
📜 SIMILAR VOLUMES
We report a phase separation study on high-quality single crystals of La2CuO4+x for two concentrations x= 0.03 and x= 0.04. The excess oxygen was loaded into the crystals at high oxygen pressure p= 3 kbar and temperature T= 650-700°C. The X-ray diffraction study of these crystals shows the presence
The diamagnetism of superconductivity and the resistivity were measured on (Lal\_xBax)2Cu04 under pressures up to 20 kbar. It was confirmed that the superconducting transition temperature T¢ is markedly restored as the resistive increment associated with the phase transition to a lowtemperature tet