Kinetics of rapeseed oil oxidation by pressure differential scanning calorimetry measurements
β Scribed by Boleslaw Kowalski; Eliza Gruczynska; Katarzyna Maciaszek
- Publisher
- John Wiley and Sons
- Year
- 2000
- Tongue
- English
- Weight
- 85 KB
- Volume
- 102
- Category
- Article
- ISSN
- 1438-7697
No coin nor oath required. For personal study only.
β¦ Synopsis
Kinetics of rapeseed oil oxidation by pressure differential scanning calorimetry measurements
Samples of rapeseed oils were oxidized at isothermal conditions in the cell of a pressure differential scanning calorimeter (PDSC). The experiments were carried out under 1400 kPa oxygen pressure at a temperature in the range of 113-144 Β°C. From resulting PDSC exotherms the times to reach the peak maximum (Ο max ) were determined and used for the assessment of the oxidative stabilities of the samples. As PDSC exotherms were obtained at different temperatures, equations for extrapolation of the Ο max values were proposed and activation energies as well as specific rate constants for oxidation were calculated.
π SIMILAR VOLUMES