Isothermal crystallization kinetics of polypropylene by differential scanning calorimetry. I. Experimental conditions

✍ Scribed by Fernando Hernández-Sánchez; Luis F. del Castillo; Ricardo Vera-Graziano


Publisher
John Wiley and Sons
Year
2004
Tongue
English
Weight
178 KB
Volume
92
Category
Article
ISSN
0021-8995

No coin nor oath required. For personal study only.


📜 SIMILAR VOLUMES


Thermal properties and isothermal crysta
✍ Pitt Supaphol; Joseph E. Spruiell 📂 Article 📅 2000 🏛 John Wiley and Sons 🌐 English ⚖ 265 KB 👁 1 views

Isothermal crystallization and subsequent melting behavior of five samples of syndiotactic polypropylene are presented. Crystallization studies were carried out in the temperature range of 60°C to 97.5°C using a differential scanning calorimeter (DSC). Subsequent DSC scans of isothermally crystalliz

Isothermal crystallization of concentrat
✍ Pascale De Meuter; Jo Amelrijckx; Hubert Rahier; Bruno Van Mele 📂 Article 📅 1999 🏛 John Wiley and Sons 🌐 English ⚖ 231 KB 👁 1 views

The slow isothermal crystallization of concentrated amorphous starch systems is measured by Modulated Differential Scanning Calorimetry (MDSC). It can be followed continuously by the evolution (stepwise decrease) of the MDSC heat capacity signal (Cp), as confirmed with data from X-ray diffractometry