Critical currents J c ðT ; BÞ for virgin and four 235 U doped Bi2223/Ag tapes irradiated with thermal neutrons (U/n treated) were measured in the temperature range T P 50 K and magnetic field B 6 1 T. Below 97 K vortex pinning in U/ n treated tapes increases with matching field B / , as evidenced by
Irreversibility fields and pinning potentials in U/n treated Bi2223/Ag tapes
✍ Scribed by I. Kušević; E. Babić; D. Marinaro; S.X. Dou; R. Weinstein
- Publisher
- Elsevier Science
- Year
- 2004
- Tongue
- English
- Weight
- 244 KB
- Volume
- 408-410
- Category
- Article
- ISSN
- 0921-4534
No coin nor oath required. For personal study only.
📜 SIMILAR VOLUMES
The measured self-field a.c. losses in mono-and multi-filamentary tapes with varying transport current, frequency and voltage tap configurations are compared to theoretical models. The observed losses are found to approach asymptotic values when the loop of the voltage taps is comparable to the widt
Experiments showing hysteresis of critical currents versus the external magnetic field I,(&.) were performed with two multifilamentary Bi(2223)/Ag tapes. The I,(&) hysteresis is observable in the transversal as well as in the longitudinal orientation of the long axis of the tape with respect to the