𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Iodine stress corrosion cracking of Zircaloy reactor cladding: iodine chemistry (a review)

✍ Scribed by P.S Sidky


Book ID
108346180
Publisher
Elsevier Science
Year
1998
Tongue
English
Weight
370 KB
Volume
256
Category
Article
ISSN
0022-3115

No coin nor oath required. For personal study only.