Intrinsic Defects in Palladium after Severe Plastic Deformation
β Scribed by Rempel, A.A. ;Nazarova, S.Z. ;Gusev, A.I.
- Publisher
- John Wiley and Sons
- Year
- 2000
- Tongue
- English
- Weight
- 62 KB
- Volume
- 181
- Category
- Article
- ISSN
- 0031-8965
No coin nor oath required. For personal study only.
π SIMILAR VOLUMES
## Dedicated to Professor Dr. Wolfgang Schro Γ ter on the occasion of his 65th anniversary The properties of multi-vacancy and multi-interstitial defects that possess luminescent bands around 1 eV are reviewed. Prominent among these are the hexavacancy and tri-and tetra-selfinterstitial defects. I