The influence of Mn compared to that of
โœ J. Degerbeck ๐Ÿ“‚ Article ๐Ÿ“… 1978 ๐Ÿ› John Wiley and Sons ๐ŸŒ German โš– 919 KB

## Abstract A large number of production and laboratory heats in grades AISI 304 and 316 with normal and extremely low managanese and sulphur contents and a number of production heats in more highly alloyed austenitic stainless steels have been studied with regard to their resistance to initiation