An acoustic emission technique for monitoring pitting corrosion of austenitic stainless steels

โœ Scribed by H. Mazille; R. Rothea; C. Tronel


Book ID
115847946
Publisher
Elsevier Science
Year
1995
Tongue
English
Weight
763 KB
Volume
37
Category
Article
ISSN
0010-938X

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES


Determination of upper Boundary pitting
โœ P. Eskelinen; O. Forsรฉn; H. Spรคhn; S. Ylรคsaari ๐Ÿ“‚ Article ๐Ÿ“… 1992 ๐Ÿ› John Wiley and Sons ๐ŸŒ German โš– 616 KB

## Abstract In this study Mode IVโ€corrosion fatigue (CF) characterized by additional superposition of pitting corrosion was investigated. Corrosion fatigue and polarization experiments were carried out on three austenitic (17Crโ€“13Niโ€“5Moโ€“0.15N, 25Niโ€“20Crโ€“5Moโ€“1.5Cu and 18Crโ€“10Niโ€“2Moโ€“0.5Ti) stainless