Stress corrosion cracking behaviour of A
✍
R. Braun
📂
Article
📅
2004
🏛
John Wiley and Sons
🌐
German
⚖ 364 KB
The stress corrosion cracking (SCC) behaviour of 8090-T8171 plate material was investigated in short transverse direction performing constant load tests and constant extension rate tests under permanent immersion conditions. At an applied stress of 100 MPa, smooth round tensile specimens were expose