Influence of Shot Peening Pressure on Stress Corrosion Susceptibility of 304 Austenitic Stainless Steel

โœ Scribed by Lu, Zhi Ming; Gao, Hong Gang; Zhu, Cheng Hui


Book ID
121247610
Publisher
Trans Tech Publications, Ltd.
Year
2012
Tongue
English
Weight
622 KB
Volume
486
Category
Article
ISSN
1662-8958

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES


Plasma nitriding of AISI 304 austenitic
โœ Lie Shen; Liang Wang; Yizuo Wang; Chunhua Wang ๐Ÿ“‚ Article ๐Ÿ“… 2010 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 943 KB

AISI 304 austenitic stainless steel was plasma nitrided at the temperature ranging from 410 to 520 ยฐC with pre-shot peening. The structural phases, micro-hardness and electrochemical behavior of the nitrided layer were investigated by optical microscopy, X-ray diffraction, micro-hardness testing and

The effect of shot peening on stress cor
โœ Y.F. Al-Obaid ๐Ÿ“‚ Article ๐Ÿ“… 1995 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 509 KB

In this paper an attempt has been made to study the effect of shot peening on stress corrosion cracking of 2205-Duplex stainless steel. Cast steel shot was selected to be the peening media. Specimens of 2205-Duplex stainless steel were tested in the peened and unpeened condition. Quantitative data o