Influence of post-annealing on the structure and optical properties of ferromagnetic Zn1−xMnxO film prepared by PECVD technique

✍ Scribed by Y.B. Lin; Y.M. Yang; G.Y. Zhao; W. Chen; Z.G. Huang


Publisher
Elsevier Science
Year
2010
Tongue
English
Weight
500 KB
Volume
405
Category
Article
ISSN
0921-4526

No coin nor oath required. For personal study only.


📜 SIMILAR VOLUMES


Influence of preparation technique on th
✍ S A Al Kuhaimi 📂 Article 📅 1998 🏛 Elsevier Science 🌐 English ⚖ 789 KB

CdS films were prepared by three different techniques-vacuum evaporation (VE), screen printing (SP), and chemical bath deposition (CBD). The influence of the preparation technique on the structural, optical and electrical properties of the polycrystalline CdS films was investigated using X-ray diffr

Effect of annealing temperature on the s
✍ Georgi P. Daniel; V.B. Justinvictor; Prabitha B. Nair; K. Joy; Peter Koshy; P.V. 📂 Article 📅 2010 🏛 Elsevier Science 🌐 English ⚖ 339 KB

ZnO thin films were deposited on corning glass substrates by RF magnetron sputtering at room temperature. The dependence of crystal structure, morphology and optical properties on postdeposition annealing was investigated using XRD, AFM and UV-vis Spectrophotometer. The asdeposited films were amorph

Oxygen flux influence on the morphologic
✍ S.C. Su; Y.M. Lu; Z.Z. Zhang; B.H. Li; D.Z. Shen; B. Yao; J.Y. Zhang; D.X. Zhao; 📂 Article 📅 2008 🏛 Elsevier Science 🌐 English ⚖ 657 KB

The Zn 1Àx Mg x O thin films were grown on Al 2 O 3 substrate with various O 2 flow rates by plasma-assisted molecular beam epitaxy (P-MBE). The growth conditions were optimized by the characterizations of morphology, structural and optical properties. The Mg content of the Zn 1Àx Mg x O thin film i

Investigations on the structural and opt
✍ C. Ravichandran; G. Srinivasan; Craig Lennon; S. Sivanathan; J. Kumar 📂 Article 📅 2010 🏛 Elsevier Science 🌐 English ⚖ 172 KB

Pure and doped zinc oxide thin films have been deposited on sapphire substrates by using the sol-gel method and spin coating technique. The X-ray diffraction pattern showed that the deposited films exhibit hexagonal zinc oxide structure. Room temperature photoluminescence measurements show the prese