Poly(ary1 ether phtha1azine)s were found to undergo an exothermic reaction at a temperature range of 360-44OOC. We elucidated the origin of the exothermic reaction and the physiochemical phenomena associated with it, based on thermal analyses, model compound studies, and 13C solid-state NMR studies.
Highly phenylated poly(aryl ether phthalazine)s
โ Scribed by Edmund Elce; Allan S. Hay
- Publisher
- John Wiley and Sons
- Year
- 1996
- Tongue
- English
- Weight
- 645 KB
- Volume
- 34
- Category
- Article
- ISSN
- 0887-624X
No coin nor oath required. For personal study only.
๐ SIMILAR VOLUMES
Several kinds of commercially available polymers of the type poly(oxy-1,4-phenylenecarbonyl-1,4-phenylene) were sulfonated by reaction with mixtures of sulfuric acid and oleum. The ether/carbonyl group ratio of the polymer chain varied from 0.67 to 2.0. With decreasing amounts of ether links in the
The synthesis of a new A 2 X-type difluoride monomer, N-2-pyridyl-4ะ,4ะ-bis-(4-fluorobenzenesulfonyl)-o-terphenyl-3,6-dimethyl-4,5-dicarboxylic imide (3), is described. The monomer 3 was incorporated into a series of copoly(aryl ether sulfone)s by polymerization of 4,4ะ-isopropylidenediphenol and 4,
A new series of aromatic heterocyclic poly(ary1 pyromellitimide-ether)s have been synthesized from various disodium metal bisphenolate salts with an N,N-bis(p-nitro-pheny1)pyromellitimide via aromatic nitro displacement solution polycondensation in dipolar aprotic solvent at elevated temperature. Th