𝔖 Bobbio Scriptorium
✦   LIBER   ✦

High temperature creep in a 〈001〉 single crystal nickel-base superalloy

✍ Scribed by P.J. Henderson; J. Lindblom


Book ID
114387848
Publisher
Elsevier Science
Year
1997
Tongue
English
Weight
398 KB
Volume
37
Category
Article
ISSN
1359-6462

No coin nor oath required. For personal study only.