๐”– Bobbio Scriptorium
โœฆ   LIBER   โœฆ

Dynamic steady-state tertiary creep in a Nickel-base single crystal superalloy at high temperatures

โœ Scribed by Nirmal K. Sinha


Publisher
Springer
Year
2005
Tongue
English
Weight
360 KB
Volume
41
Category
Article
ISSN
0022-2461

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES


Anisothermal creep behavior at very high
โœ J. Cormier; X. Milhet; J. Mendez ๐Ÿ“‚ Article ๐Ÿ“… 2008 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 438 KB

Nickel-based superalloy single crystal specimens have been tested under anisothermal creep conditions using two different routes, both including an overheating stage. In the first route, the material is tested under creep conditions at 1050 โ€ข C, then submitted to an overheating regime at 1200 โ€ข C, a