Fatigue small crack growth in a single crystal nickel-base superalloy at elevated temperature: Okazaki, M., Imai, T., Satoh, T. and Nohmi, S. J. Soc. Mater. Sci. Jpn (Aug. 1992) 41 (467) 1261–1267 (in Japanese)