Recrystallization and grain-growth behav
Recrystallization and grain-growth behavior of a nickel-base superalloy during multi-hit deformation
โ
D.S. Weaver; S.L. Semiatin
๐
Article
๐
2007
๐
Elsevier Science
๐
English
โ 230 KB