Nickel self-diffusion along grain bounda
โœ N.P. Zulina; E.V. Bolberova; I.M. Razumovskii ๐Ÿ“‚ Article ๐Ÿ“… 1996 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 805 KB

63Ni self-diffusion along grain boundaries (GBs) in intermetallic alloys Ni-25.2A1, Ni-24.9A14.8W, Ni-24.2A14.7Cr, Ni-19.3A14.5Hf and Ni-27.6Al-4.9Co (at.%) has been investigated by the radiotracer technique. The usual darkening in the positions of GBs on the autoradiographs obtained on the parallel

Accelerated diffusion of hydrogen along
โœ A.M. Brass; A. Chanfreau ๐Ÿ“‚ Article ๐Ÿ“… 1996 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 991 KB

Accelerated diffusion of hydrogen was observed at room temperature in polycrystalline nickel samples with the electrochemical permeation technique. A larger hydrogen flux was measured in annealed samples with 25 pm grain size whereas faster hydrogen diffusion was observed at the early stage of the p