Grain boundary wetting in ceramic cuprates

✍ Scribed by V. V. Belousov


Publisher
Springer
Year
2005
Tongue
English
Weight
653 KB
Volume
40
Category
Article
ISSN
0022-2461

No coin nor oath required. For personal study only.


πŸ“œ SIMILAR VOLUMES


Finite size scaling in grain boundary we
✍ V. Traskine; P. Volovitch; L. Barrallier; Ya. Kucherinenko; P. Protsenko; Z. Skv πŸ“‚ Article πŸ“… 2005 πŸ› Springer 🌐 English βš– 716 KB
Wetting transition of grain-boundary tri
✍ B.B. Straumal; O. Kogtenkova; P. ZiΔ™ba πŸ“‚ Article πŸ“… 2008 πŸ› Elsevier Science 🌐 English βš– 732 KB

The wetting phase transition of grain boundaries (GBs) and grain-boundary triple junctions (GB TJs) by the melt has been studied in the Al-30 wt.%Zn and Al-10 wt.%Zn-4 wt.%Mg polycrystals. The condition of complete wetting is weaker for TJs (r GB > ffiffi ffi 3 p r SL ) than that for GBs (r GB > 2r

Solid-state wetting transitions at grain
✍ Paul Wynblatt; Dominique Chatain πŸ“‚ Article πŸ“… 2008 πŸ› Elsevier Science 🌐 English βš– 695 KB

A previously developed model of the dependence of grain boundary (GB) segregation on GB character has been exercised to investigate solidstate wetting transitions at GBs, and their anisotropy. In the case of binary systems displaying a solid-state miscibility gap, it is shown that the wetting transi

Grain boundary mobility and grain growth
✍ Byung-Kwon Yoon; Si-Young Choi; Takahisa Yamamoto; Yuichi Ikuhara; Suk-Joong L. πŸ“‚ Article πŸ“… 2009 πŸ› Elsevier Science 🌐 English βš– 742 KB

The effect of an intergranular amorphous film on grain growth behavior has been studied in a faceted model system, BaTiO 3 . We prepared two kinds of samples with and without intergranular amorphous films but with the same grain size and density. During annealing the samples at 1350 Β°C in air, abnor

Pressure effect on grain boundary wettin
✍ E. I. Rabkin; W. Gust; W. Łojkowski; V. Paidar πŸ“‚ Article πŸ“… 1994 πŸ› Springer 🌐 English βš– 419 KB

Bicrystals of Fe-6 at.% Si alloy containing (001){001}$5 tilt grain boundaries with a deposited zinc layer have been annealed at various hydrostatic pressure at four temperatures between 700 ~ and 905~ After the anneals the dihedral angle 0 of the grain boundary groove formed at the site of the grai