Differential scanning calorimetry was used to investigate the glass-to-rubber transition at 383 K of Illinois No. 6 coal dried at 383 K and thermally treated to 523 K. The intensity of the transition is 0.2 J g-' K-I, 'run 2' in Figure 1. The sample was then cooled to 303 K. This procedure was repea
Glass transition and enthalpy relaxation of amorphous lactose glass
โ Scribed by Md. Kamrul Haque; Kiyoshi Kawai; Toru Suzuki
- Book ID
- 108080365
- Publisher
- Elsevier Science
- Year
- 2006
- Tongue
- English
- Weight
- 279 KB
- Volume
- 341
- Category
- Article
- ISSN
- 0008-6215
No coin nor oath required. For personal study only.
๐ SIMILAR VOLUMES
Thermal transition of cross-linked corn starches was characterized by using a differential scanning calorimeter (DSC) in the presence of excess (67%, based on total weight) or limited (15%) water. Normal corn starch (, 24% amylose) was cross-linked by reacting with a mixture (99:1) of sodium trimeta
Coal tar pitches generally have very complex chemical compositions and structures. Their physico-chemical properties depend on the mutual molecular interactions of their various components. In order to characterize these materials further the properties related to their glass transition behaviour ha