## Abstract The way in which the stationary potential of a zinc electrode previously treated with various passivating and inhibiting solutions changes in the present of the chloride, bromide and iodide ions is studied in solutions of potassium chromate, disodium hydrogen phosphate and sodium tungst
Galvanic Corrosion in the Copper/Zinc System: I. Potential distribution in relation to the nature of the cathode and to the type of anion in solution
β Scribed by El Din, A. M. Shams; El Kader, J. M. Abd; Badran, M. M.
- Book ID
- 127091373
- Publisher
- Institute of Materials, Minerals and Mining
- Year
- 1981
- Tongue
- English
- Weight
- 456 KB
- Volume
- 16
- Category
- Article
- ISSN
- 0007-0599
No coin nor oath required. For personal study only.
π SIMILAR VOLUMES
This research produced statistically based, semimechanistic models describing partitioning of Cu and Zn in 40 soils from the United States, Canada, the United Kingdom (UK), The Netherlands, and Chile with widely varying characteristics. Two different types of models were constructed, partitioning mo
## Abstract Potentiodynamic anodic polarization curves have been traced for an electrode of the steel Deltaβ52 (0.40, 0.78Mn, 0.045 S, 0.06P, 0.23 Si): the aggresive media used were potassium hydroxide without and with additions of potassium chloride, bromide and iodide. The oxide film present on t