Fracture of sustained tensile-loaded Ti–0.2% Pd alloy in acid and neutral fluoride solutions

✍ Scribed by Ken’ichi Yokoyama; Toshio Ogawa; Kenzo Asaoka; Jun’ichi Sakai


Book ID
104061228
Publisher
Elsevier Science
Year
2006
Tongue
English
Weight
728 KB
Volume
419
Category
Article
ISSN
0921-5093

No coin nor oath required. For personal study only.


📜 SIMILAR VOLUMES


Fracture associated with hydrogen absorp
✍ Yokoyama, Ken'ichi ;Kaneko, Kazuyuki ;Miyamoto, Youji ;Asaoka, Kenzo ;Sakai, Jun 📂 Article 📅 2003 🏛 John Wiley and Sons 🌐 English ⚖ 407 KB

## Abstract The fracture of commercial pure titanium in acid and neutral fluoride solutions has been examined by a sustained tensile‐loading test and hydrogen thermal desorption analysis. It was found that the fracture of titanium occurred in neutral 2.0% NaF solution as well as in 2.0% acidulated

Delayed fracture of Ni-Ti superelastic a
✍ Yokoyama, Ken'ichi ;Kaneko, Kazuyuki ;Moriyama, Keiji ;Asaoka, Kenzo ;Sakai, Jun 📂 Article 📅 2004 🏛 John Wiley and Sons 🌐 English ⚖ 479 KB

## Abstract Hydrogen‐related degradation of the mechanical properties of a Ni‐Ti superelastic alloy has been examined by means of delayed fracture tests in acidic and neutral fluoride solutions and hydrogen thermal desorption analysis. Delayed fracture took place in both solutions; the time to frac

Fracture of Ni-Ti superelastic alloy und
✍ Ken'ichi Yokoyama; Toshio Ogawa; Atsushi Fujita; Kenzo Asaoka; Jun'ichi Sakai 📂 Article 📅 2007 🏛 John Wiley and Sons 🌐 English ⚖ 572 KB

## Abstract The fracture of Ni‐Ti superelastic alloy has been investigated by a sustained tensile‐loading test in physiological saline solution containing hydrogen peroxide (0.15__M__ NaCl + 0.3__M__ H~2~O~2~). The fracture always occurs when the applied stress exceeds the critical stress for marte