FATIGUE, CREEP AND CREEP/FATIGUE BEHAVIOUR OF A NICKEL BASE SUPERALLOY AT 700°C

✍ Scribed by T. H. Hyde; L. Xia; A. A. Becker; W. Sun


Book ID
109013866
Publisher
John Wiley and Sons
Year
1997
Tongue
English
Weight
572 KB
Volume
20
Category
Article
ISSN
8756-758X

No coin nor oath required. For personal study only.


📜 SIMILAR VOLUMES


Creep of PE-10 nickel-base superalloy at
✍ A. J. Marzocca; A. C. Picasso 📂 Article 📅 1994 🏛 Springer 🌐 English ⚖ 853 KB

Creep data, at 973 K and stresses between 355 and 512 MPa, in flat specimens of PE-IO nickel-base superalloy are reported. The data have been interpreted in terms of a constitutive equation based on a creep model involving dislocation climb and cross-slip over the strengthening phase. Strain-rate se