Electrochemical Investigations of Pitting Corrosion in Nitrogen-Bearing Type 316LN Stainless Steel

✍ Scribed by Palit, G. C.; Kain, V.; Gadiyar, H. S.


Book ID
120473160
Publisher
NACE International
Year
1993
Tongue
English
Weight
169 KB
Volume
49
Category
Article
ISSN
0010-9312

No coin nor oath required. For personal study only.


πŸ“œ SIMILAR VOLUMES


Hydrogen effects on pitting corrosion an
✍ S. Ningshen; U. Kamachi Mudali πŸ“‚ Article πŸ“… 2009 πŸ› Elsevier Science 🌐 English βš– 976 KB

The effects of hydrogen pre-charging on pitting corrosion resistance and semiconducting nature of passive film formed on two different nitrogen-containing type 316L stainless steel (0.076 and 0.086 wt% N) have been studied. Auger electron spectroscopy (AES) analysis of the alloys after passivation i