The growth kinetics of passive films on Fe, Fe-10 Ni, Fe10 Cr, Fe-10 Ni-10 Cr have been determin ed in pH 8.4 borate buffer solution at 25°C using ellipsometer and coulometric techniques. Films found on the alloys were progressively thinner as the alloy concentration was increased. The correlations
✦ LIBER ✦
Electrical resistivity of FeCr- and NiCr-based amorphous alloys
✍ Scribed by D.F. Jones; G. Stroink; Z.M. Stadnik; R.A. Dunlap
- Publisher
- Elsevier Science
- Year
- 1988
- Weight
- 248 KB
- Volume
- 99
- Category
- Article
- ISSN
- 0025-5416
No coin nor oath required. For personal study only.
📜 SIMILAR VOLUMES
Growth kinetics of passive films on Fe,
✍
K.N. Goswami; R.W. Staehle
📂
Article
📅
1971
🏛
Elsevier Science
🌐
English
⚖ 928 KB
Structures and properties of rapidly sol
✍
C.N. Elliot; H.A. Davies; G.W. Greenwood
📂
Article
📅
1988
🏛
Elsevier Science
⚖ 447 KB
Viscoplastic properties of an FeCrPC
✍
A. Bouali; C. Tete
📂
Article
📅
1988
🏛
Elsevier Science
⚖ 245 KB
Damage recovery in electron-irradiated F
✍
Amdulla O.O. Mekhrabov; Eiichi Sato; Michio Shimotomai; Masao Doyama; Tadao Iwat
📂
Article
📅
1985
🏛
Elsevier Science
🌐
English
⚖ 381 KB
Neutron irradiation of FeMn, FeCrMn a
✍
F.A. Garner; H.R. Brager; D.S. Gelles; J.M. McCarthy
📂
Article
📅
1987
🏛
Elsevier Science
🌐
English
⚖ 788 KB
The low temperature magnetic properties
✍
L.A.A. Warnes; H.W. King
📂
Article
📅
1981
🏛
Elsevier Science
🌐
English
⚖ 271 KB
The magnetic properties of ternary Fe-Cr-Ni alloys containing 17 wt% Ni and 18-24 wt% Cr have been studied over a range of temperatures from 4.2 -35 K by both ac and dc techniques in fields from 5 Am-1 \_ 6 MA m-1. A t room temperature, the matrix of all the alloys was the paramagnetic fcc austenite