Effects of the behaviour of the proton-induced isotopes production on the analysis of ancient alloys
β Scribed by G. Pappalardo; A. Esposito; G.A. Cirrone; G. Cuttone; S. Garraffo; L. Pappalardo; F. Rizzo; F.P. Romano; S. Russo
- Publisher
- Elsevier Science
- Year
- 2008
- Tongue
- English
- Weight
- 906 KB
- Volume
- 266
- Category
- Article
- ISSN
- 0168-583X
No coin nor oath required. For personal study only.
β¦ Synopsis
The present work concerns non-destructive ion beam analysis carried out by means of proton-beam-induced nuclear reactions in the 10-30 MeV energy range. We focused our attention on the yield distribution of the isotopes produced in the internal region of a metal alloy. This distribution, which defines the analytical region, displays, at incident energy of about 20 MeV in a bronze based alloy, a bellshaped curve centred at about 600 lm with an average width of about 400 lm. By changing the incident proton energy it is possible to displace the above region in the interior of the metal body. It should be pointed out that if we neglect to take into account the correct behaviour of the isotope yield distribution in samples with surface inhomogeneities we can obtain erroneous analytical results. We describe some experiments based on proton activation analysis (PAA) carried out at the INFN-Laboratori Nazionali del Sud (LNS) in Catania where we verified the bell-shape of the radioactive isotope distribution. The resulting formulas are given for quantitative analysis.
It is straightforward that, by choosing the appropriate incident proton energy, it is possible to confine the whole analytical region to the interior of the body, thus eliminating any influence of surface effects. We have called this particular approach deep proton activation analysis (DPAA). Examples of its use on archaeological artefacts are given.
π SIMILAR VOLUMES
## Abstract The effects of yttrium additions on the oxidation behaviour of Feβ20Crβ5Al(wt%) alloys have been investigated in oxidation tests and cyclic heatingβelement tests at temperatures ranging from 1100 to 1400Β°C in air. Experimental results showed that the oxidation resistance of the alloys d
The stress corrosion cracking behaviour of plate material of the aluminium alloys 2024-T351, 8090-T8171, 7475-T651, and 7075-T7351 was investigated performing constant load tests. Short transverse tensile specimens were permanently immersed in aerated aqueous 0.6 M Na 2 Cl solutions with additions o