𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Effect of structure on stress corrosion cracking of nitrogen-alloyed high-strength 05Kh15N4AM2 steel

✍ Scribed by Z. N. Petropavlovskaya; E. V. Kuznetsov; I. L. Kharina; I. A. Guseva; M. S. Petrova; P. Lengarski; Ch. Andreev


Publisher
Springer
Year
1992
Tongue
English
Weight
205 KB
Volume
28
Category
Article
ISSN
1573-885X

No coin nor oath required. For personal study only.