𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Effect of stress corrosion cracking on stress–strain response of steel wires used in prestressed concrete beams

✍ Scribed by Ngoc Anh Vu; Arnaud Castel; Raoul François


Book ID
116385240
Publisher
Elsevier Science
Year
2009
Tongue
English
Weight
788 KB
Volume
51
Category
Article
ISSN
0010-938X