Effect of crack tip stress intensity on the mechanism of stress-corrosion cracking of titanium-6a-4V in methanol

โœ Scribed by D.A. Meyn


Book ID
117086383
Publisher
Elsevier Science
Year
1967
Tongue
English
Weight
420 KB
Volume
7
Category
Article
ISSN
0010-938X

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES


Effect of curvature at the crack tip on
โœ Nao-Aki Noda; Kazuhiro Oda ๐Ÿ“‚ Article ๐Ÿ“… 1993 ๐Ÿ› Springer Netherlands ๐ŸŒ English โš– 485 KB

In this paper, the numerical solution of the hypersingular integral equation using the body force method in cucved crack problems is presented. In the body force method, the stress fields induced by two kinds of standard set of force doublets are used as fundamental solutions. Then, the problem is f

Effect of a hole near a crack tip on the
โœ Chen Yi-Heng ๐Ÿ“‚ Article ๐Ÿ“… 1986 ๐Ÿ› Springer Netherlands ๐ŸŒ English โš– 155 KB

A partitioning plan combined with the generalized variational method is presented for studying the effect of a hole near a crack tip on the stress intensity factor. The hole is at an arbitrary distance relative to the crack tip and the influence of the distance is determined numerically. Consider