Kinetic effect of boron on the thermal s
β
A.H. Tavakoli; P. Gerstel; J.A. Golczewski; J. Bill
π
Article
π
2010
π
Elsevier Science
π
English
β 890 KB
The isothermal mass loss of two polymer-derived ceramics with compositions SiC 1.4 N 0.9 and SiC 1.5 N 1.0 B 0.05 were measured as a function of time using thermal gravimetric analysis at various temperatures ranging between 1580 and 1720 Β°C. The process of mass loss, attributed to the reaction Si 3