Studies on void coalescence analysis of
โ
N. Naga Krishna; A.K. Akash; K. Sivaprasad; R. Narayanasamy
๐
Article
๐
2010
๐
Elsevier Science
โ 624 KB
Cryorolling was performed on commercially pure aluminium sheet from an initial thickness of 7 mm to 0.25 mm with a total true strain of around 3.33. Cryorolling was performed in many passes with only 5% reduction in each pass to avoid adiabatic heating during rolling process. Detailed Transmission E