๐”– Bobbio Scriptorium
โœฆ   LIBER   โœฆ

Dynamic Responses of Nickel-Based Single Crystal Superalloy DD6 Blade

โœ Scribed by Yingwu Fang, Yinghong Li


Book ID
120946428
Publisher
Springer US
Year
2012
Tongue
English
Weight
678 KB
Volume
22
Category
Article
ISSN
1059-9495