Nanoindentation is modelled on the computer by means of a simple two-dimensional discrete dislocation model in order to study the influence of the orientation of predefined slip bands on certain phenomena, which often occur during real indentation experiments, systematically. By assuming single slip
β¦ LIBER β¦
Discrete dislocation simulation of nanoindentation: the effect of moving conditions and indenter shape
β Scribed by H.G.M. Kreuzer; R. Pippan
- Publisher
- Elsevier Science
- Year
- 2004
- Tongue
- English
- Weight
- 103 KB
- Volume
- 387-389
- Category
- Article
- ISSN
- 0921-5093
No coin nor oath required. For personal study only.
π SIMILAR VOLUMES
Discrete dislocation simulation of nanoi
β
H.G.M. Kreuzer; R. Pippan
π
Article
π
2007
π
Elsevier Science
π
English
β 759 KB
Discrete dislocation simulation of nanoi
β
H.G. M. Kreuzer; R. Pippan
π
Article
π
2005
π
Elsevier Science
π
English
β 199 KB
Finite element simulation of the effect
β
C. Walter; T. Antretter; R. Daniel; C. Mitterer
π
Article
π
2007
π
Elsevier Science
π
English
β 440 KB
Effect of State on the Shape of the Disl
β
V. B. Pariiskii
π
Article
π
1967
π
John Wiley and Sons
π
English
β 480 KB
Discrete Element Method Simulation of Ef
β
M. Khanal; R. Raghuramakrishnan; J. Tomas
π
Article
π
2008
π
John Wiley and Sons
π
English
β 325 KB
The effect of box shape on the dynamic p
β
Tsjerk A. Wassenaar; Alan E. Mark
π
Article
π
2005
π
John Wiley and Sons
π
English
β 362 KB
π 1 views
## Abstract The effect of the box shape on the dynamic behavior of proteins simulated under periodic boundary conditions is evaluated. In particular, the influence of simulation boxes defined by the nearβdensest lattice packing (NDLP) in conjunction with rotational constraints is compared to that o