The stored energy of cold work and its r
β
A.L Titchener; M.B Bever
π
Article
π
1960
π
Elsevier Science
β 632 KB
One set of wires of an 82.6 Au-17.4 Ag (wt.%) alloy was drawn at -195Β°C to a true strain of 0.62. A second set, after drawing at -195Β°C to a strain of 0.62, was annealed at room temperature. Two further sets were drawn at -195Β°C to a strain of 0.62, brought to room temperature and drawn to total st