Differential scanning calorimetric studies of ferroelectric rare-earth molybdates

✍ Scribed by M. Roy; R.N.P. Choudhary; H.N. Acharaya


Publisher
Elsevier Science
Year
1989
Tongue
English
Weight
442 KB
Volume
145
Category
Article
ISSN
0040-6031

No coin nor oath required. For personal study only.


πŸ“œ SIMILAR VOLUMES


Differential scanning calorimetric studi
✍ Marie-Madeleine SacrΓ©; Winfried Hoffmann; Margaret Turner; Jean-Francois Tocanne πŸ“‚ Article πŸ“… 1979 πŸ› Elsevier Science 🌐 English βš– 630 KB

Differential scanning calorimetric studies have been made of some pure phosphatidyl glycerol (PG) lipid-water systems. The influence of pH, salt concentration and the monovalent cations (Na Γ·, K + and NH, Γ·) upon the lipid phase transitions have been studied. The calorimetric data is compared with c