Deformation and strength characteristics of magnesia-spinnellide refractories at elevated temperatures
โ Scribed by R. A. Panfilov; V. M. Ustyantsev; T. I. Remezova; S. P. Postnikova; M. Ya. Landa; V. V. Nikolaev
- Publisher
- Springer US
- Year
- 1991
- Tongue
- English
- Weight
- 289 KB
- Volume
- 32
- Category
- Article
- ISSN
- 1573-9139
No coin nor oath required. For personal study only.
๐ SIMILAR VOLUMES
The dynamic yield and fracture stress of two refractory alloys were measured under shock-wave loading at normal and elevated (up to 680 C) temperatures. The tested materials were polycrystalline nickel-based superalloy Inconel IN738LC and PWA 1483 Ni-Co-Fe alloy in quasi-monocrystalline state. Both
Experimental data relating to standard rates of loading are studied on concrete control specimens 28 days after casting. Normal concrete with an oven-dry density in the range 2000-2800 kg/m3 is used for the specimens. The rates of compression are about 0.3 N/mm\*/sec, or a strain rate of about 30 x