Assessment of moisture content in nylon using differential scanning calorimetry

โœ Scribed by C.Y. Yue; C.Y. Chan


Publisher
Elsevier Science
Year
1991
Tongue
English
Weight
295 KB
Volume
10
Category
Article
ISSN
0142-9418