Apatite formation on (2 − x)CaO·x3 M2O3·2SiO2 glasses (M = La, Y; 0 ⩽ x ⩽ 0.6) in a simulated body fluid
✍ Scribed by R. Fresa; A. Costantini; A. Buri; F. Branda
- Publisher
- Elsevier Science
- Year
- 1995
- Tongue
- English
- Weight
- 654 KB
- Volume
- 16
- Category
- Article
- ISSN
- 0142-9612
No coin nor oath required. For personal study only.
📜 SIMILAR VOLUMES
We present high resolution inelastic neutron scattering measurements of the linewidths of crystal field transitions in Tm0.1Y0 9Ba2Cu306÷x, which are proportional to the local magnetic response of the Cue 2 planes at t'lie traiisition energies, 12 to 14 meV. There is no change in the magnitude ot th
Nb and Ta substitutions in YBa2Cu307 and related phases have been examined in an attempt to synthesise phases of formula LBa2Cu2MOs (L = rare earth, M = Nb, Ta), in which the square planar Cu I sites of the YBa2Cu307 structure are occupied by M, and complete oxygen occupancy in the basal plane of th