Anodic oxidation of indium phosphide in glycol-based solutions
β Scribed by Alexander Colquhoun; Hans L. Hartnagel
- Publisher
- Elsevier Science
- Year
- 1977
- Weight
- 663 KB
- Volume
- 5
- Category
- Article
- ISSN
- 0376-4583
No coin nor oath required. For personal study only.
π SIMILAR VOLUMES
Passive 8hn growth, electrodissolution and pitting corrosion of iridium electrodes in NaCl solutions in the pH range 2-12.6 were studied using potentiostatic and potentiodynamic techniques complemented with SEM. In the pH range between 10.5 and 12.6 the oxide formation should involve a mixed control
The potential of tellurium anodes has been measured as a function of current density in 0.01-3 N NaOH at 30Β°C. The results indicate the oxidation of tellurium into tellurous acid. The initial discharge of hydroxyl ions governs the overall reaction rate within the concentration range 0.01-l N. In con