β¦ Synopsis
The amorphous phase content of air plasmasprayed hydroxyapatite coatings is dependent upon spraying and deposition conditions. X-ray diffraction and optical microscopy were used to investigate the influence of spray parameters on the formation of the amorphous phase. Results show three factors which most influence the formation of the amorphous phase: dehydroxylation of the molten particle during flight, the cooling rate as it impinges onto the metal substrate, and the substrate temperature. Crystalline regions were identified as unmelted particles and elongated recrystallized areas. Amorphous phase regions vary throughout the coating but are more commonly found at the coating-substrate interface, i.e., the regions decrease toward the surface of the coating. Such an inhomogeneous distribution of phase content is expected to affect the clinical process of bone deposition, and therefore successful implant fixation.
π SIMILAR VOLUMES
A method to measure the amorphous calcium phosphate (ACP) content of plasma sprayed hydroxyapatite (HA) coatings is presented. The areas of the crystalline peaks and the broad amorphous "hump" in an X-ray diffraction scan of a mixture of crystalline and amorphous HA can be fitted using conventional
## Abstract The clinical use of plasmaβsprayed hydroxyapatite (HA) coatings on metal implants has been widely adopted because the HA coating can achieve the firmly and directly biological fixation with the surrounding bone tissue. However, the longβterm mechanical properties of HA coatings has been
The purpose of this study was to evaluate the effect of atmo-sphere, tricalcium phosphate (TCP) and tetracalcium phossphere on the phase transformation in hydroxyapatite (HA) phate (TTCP) were more stable than HA, so heat treatcoatings during heat treatment by varying the atmosphere ment could not c