𝔖 Bobbio Scriptorium
✦   LIBER   ✦

AFM nanoindentation to determine Young’s modulus for different EPDM elastomers

✍ Scribed by R. Ferencz; J. Sanchez; B. Blümich; W. Herrmann


Book ID
113857892
Publisher
Elsevier Science
Year
2012
Tongue
English
Weight
525 KB
Volume
31
Category
Article
ISSN
0142-9418

No coin nor oath required. For personal study only.


📜 SIMILAR VOLUMES


Determining the Young's modulus and cree
✍ Kristof Wouters; Robert Puers 📂 Article 📅 2009 🏛 Elsevier Science 🌐 English ⚖ 866 KB

In this study, a fundamental measurement of the Young's modulus of Epoclad and Epocore negative photo resist is performed, using a miniature tensile test setup. The experiments were done on miniature dog bone tensile test structures which are fabricated using normal micro machining methods. In addit