The aging characteristics, elevated-temperature strength and stiffness as well as creep deformation of aluminum alloy 6061 composites reinforced with silicon carbide (SIC) whiskers (V f= 0.20) have been studied. The peak hardness for this composite was 148 kgf mm 2 after aging for 18 h at 150°C and
✦ LIBER ✦
Abrasive wear of silicon carbide particulate— and whisker-reinforced 7091 aluminum matrix composites
✍ Scribed by Wang Aiguo; H.J. Rack
- Book ID
- 107873264
- Publisher
- Elsevier Science
- Year
- 1991
- Tongue
- English
- Weight
- 958 KB
- Volume
- 146
- Category
- Article
- ISSN
- 0043-1648
No coin nor oath required. For personal study only.
📜 SIMILAR VOLUMES
Elevated-temperature mechanical properti
✍
Ram B. Bhagat; Michael B. House
📂
Article
📅
1991
🏛
Elsevier Science
🌐
English
⚖ 708 KB
Deformation behavior of silicon-carbide-
✍
R.J. Lederich; S.M.L. Sastry
📂
Article
📅
1982
🏛
Elsevier Science
⚖ 369 KB
Notched behaviour of a silicon carbide p
✍
Ze Wen Huang; Ian R. McColl; Samuel J. Harris
📂
Article
📅
1996
🏛
Elsevier Science
🌐
English
⚖ 558 KB
The notched fatigue behaviour of a fine particulate reinforced A1-Cu-Mg (2124) matrix composite is compared with that of an equivalent monolithic alloy (2024), both in the T4 condition. The difference in response of the materials for tensile and fatigue loading is pronounced. Under tensile loading t
Effect of silicon carbide particulates o
✍
S. Suresha; B.K. Sridhara
📂
Article
📅
2010
🏛
Elsevier Science
⚖ 996 KB
Evaluation of dry sliding wear behavior
✍
Sun Zhiqiang; Zhang Di; Li Guobin
📂
Article
📅
2005
🏛
Elsevier Science
⚖ 380 KB
Processing and Response of Aluminum-Lith
✍
K.A. Khor; Y. Cao; F.Y.C. Boey; K. Hanada; Y. Murakoshi; T.S. Sudarshan; T.S. Sr
📂
Article
📅
1997
🏛
Springer US
🌐
English