๐”– Bobbio Scriptorium
โœฆ   LIBER   โœฆ

A new diffusion-inhibited oxidation-resistant coating for superalloys

โœ Scribed by Michael A. Gedwill; Thomas K. Glasgow; Stanley R. Levine


Book ID
103426995
Publisher
Elsevier Science
Year
1982
Tongue
English
Weight
647 KB
Volume
95
Category
Article
ISSN
0040-6090

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES


Evaluation of aluminide diffusion coatin
โœ A. Elsawy; H. Soda; A. McLean ๐Ÿ“‚ Article ๐Ÿ“… 2005 ๐Ÿ› John Wiley and Sons ๐ŸŒ German โš– 756 KB

The cast wires were used as evaporation sources for ion-vapour deposition followed by diffusion heat treatments to form nickel aluminide coatings. In order to examine the oxidation resistance of these coatings at elevated temperatures, thermal cyclic oxidation experiments were carried out in air at

Oxidation resistance of a Zr-doped NiAl
โœ S. Hamadi; M.-P. Bacos; M. Poulain; A. Seyeux; V. Maurice; P. Marcus ๐Ÿ“‚ Article ๐Ÿ“… 2009 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 544 KB

The influence of the reactive element Zr on the oxidation behavior of the AM1/NiAl system has been investigated by means of cyclic oxidation combined with SEM microstructural characterizations and ToF-SIMS depthprofiling, and by isothermal oxidations followed by thermogravimetric analyses. Although