𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Improvement in oxidation resistance of a Ni3Al-based superalloy IC6 by rhenium-based diffusion barrier coatings

✍ Scribed by Fengqun Lang; Toshio Narita


Book ID
116574367
Publisher
Elsevier Science
Year
2007
Tongue
English
Weight
803 KB
Volume
15
Category
Article
ISSN
0966-9795