A differential scanning calorimetric study of the decomposition of some lanthanide nitrates

✍ Scribed by C.A. Strydom; C.P.J. Van Vuuren


Publisher
Elsevier Science
Year
1989
Tongue
English
Weight
515 KB
Volume
147
Category
Article
ISSN
0040-6031

No coin nor oath required. For personal study only.


πŸ“œ SIMILAR VOLUMES


Differential scanning calorimetric studi
✍ Marie-Madeleine SacrΓ©; Winfried Hoffmann; Margaret Turner; Jean-Francois Tocanne πŸ“‚ Article πŸ“… 1979 πŸ› Elsevier Science 🌐 English βš– 630 KB

Differential scanning calorimetric studies have been made of some pure phosphatidyl glycerol (PG) lipid-water systems. The influence of pH, salt concentration and the monovalent cations (Na Γ·, K + and NH, Γ·) upon the lipid phase transitions have been studied. The calorimetric data is compared with c