A Calibration Round-Robin Protocol for Nanoindentation Measurements of Thin Film Coatings

✍ Scribed by Cabibbo, M.; Spigarelli, S.


Book ID
121933760
Publisher
Elsevier
Year
2013
Tongue
English
Weight
264 KB
Volume
40
Category
Article
ISSN
1875-3892

No coin nor oath required. For personal study only.


πŸ“œ SIMILAR VOLUMES


Quantitative AES: Calibration of spectro
✍ M. P. Seah; G. C. Smith πŸ“‚ Article πŸ“… 1990 πŸ› John Wiley and Sons 🌐 English βš– 405 KB

## Abstract As a result of careful calibration, a metrology spectrometer has been developed at the National Physical Laboratory (NPL) to give true spectra. This instrument has been used to measure the true spectra from three reference materials under defined conditions in AES. Measurements for thes