๐”– Bobbio Scriptorium
โœฆ   LIBER   โœฆ

Young's modulus of polycrystalline Li12Si7 using nanoindentation testing

โœ Scribed by J.B. Ratchford; B.A. Crawford; J. Wolfenstine; J.L. Allen; C.A. Lundgren


Book ID
113748989
Publisher
Elsevier Science
Year
2012
Tongue
English
Weight
186 KB
Volume
211
Category
Article
ISSN
0378-7753

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES


Young's modulus of polycrystalline Li22S
โœ J.B. Ratchford; B.E. Schuster; B.A. Crawford; C.A. Lundgren; J.L. Allen; J. Wolf ๐Ÿ“‚ Article ๐Ÿ“… 2011 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 390 KB

In order for Li-Si alloys to be used in Li-ion batteries as anodes, knowledge of their mechanical properties, such as Young's moduli, is crucial. Young's modulus of polycrystalline Li 22 Si 5 was determined from nanoindentation testing. The value of Young's modulus was 35.4 ยฑ 4.3 GPa. This value is

Young's modulus of nanocrystalline Fe me
โœ G.E. Fougere; L. Riester; M. Ferber; J.R. Weertman; R.W. Siegel ๐Ÿ“‚ Article ๐Ÿ“… 1995 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 551 KB

Nanoindentation techniques were used to measure Young's modulus for nanocrystalline Fe samples produced by inert-gas condensation and warm consolidation. The samples had grain sizes of 4-20 nm and residual porosity of 2-30% calculated relative to conventional Fe. Values of Young's modulus for the na