The physical properties of concrete containing ground bagasse ash (BA) including compressive strength, water permeability, and heat evolution, were investigated. Bagasse ash from a sugar factory was ground using a ball mill until the particles retained on a No. 325 sieve were less than 5wt%. They we
โฆ LIBER โฆ
Utilization of bagasse ash in high-strength concrete
โ Scribed by Sumrerng Rukzon; Prinya Chindaprasirt
- Book ID
- 113784926
- Publisher
- Elsevier Science
- Year
- 2012
- Weight
- 644 KB
- Volume
- 34
- Category
- Article
- ISSN
- 0261-3069
No coin nor oath required. For personal study only.
๐ SIMILAR VOLUMES
Utilization of bagasse ash as a pozzolan
โ
Nuntachai Chusilp; Chai Jaturapitakkul; Kraiwood Kiattikomol
๐
Article
๐
2009
๐
Elsevier Science
๐
English
โ 617 KB
Utilization of high-strength concrete
โ
Ivar Holand
๐
Article
๐
1996
๐
Elsevier Science
๐
English
โ 90 KB
Utilization of Bagasse Ash as a Partial
โ
Modani, Prashant O.; Vyawahare, M.R.
๐
Article
๐
2013
๐
Elsevier
๐
English
โ 137 KB
Utilization of high-strength concrete in
โ
Hu, Qingchang ;Zhu, Zingquan
๐
Article
๐
1994
๐
John Wiley and Sons
๐
English
โ 769 KB
Long-term strength of high fly ash concr
โ
Torben C. Hansen
๐
Article
๐
1990
๐
Elsevier Science
๐
English
โ 172 KB
Five fly ash concretes were found to gain considerable strength beyond 28 days when standard cured in water at 20ยฐC. However, strength development came to an almost complete stop after 3ยฝ years, at what time the fly ash activity factors with respect to concrete compressive strength ranged from 0.86
Study on Strength Characteristics of Hig
โ
Ravande Kishore; V. Bhikshma; P. Jeevana Prakash
๐
Article
๐
2011
๐
Elsevier
๐
English
โ 458 KB